Detalhes essenciais
Envio:海运
Introdução do Produto
Low temperature container plate produced in China 15CrMoR Impact temperature 20℃
Lower yield strength ReL/MPa ≥295 (T/mm 6~60) ≥275 (T/mm 60~100) ≥255 (T/mm 100~200)
Tensile strength Rm/MPa 450~590 (T/mm 6~100) 440~580 (T/mm 100~200)
Tensile strength Rm/MPa 450~590 (T/mm 6~100) 440~580 (T/mm 100~200)
Elongation after fracture A/% ≥19
Impact absorption energy KV₂/J ≥47
Specification/mm:T (6~80+)*W*L