Essential details
Shipping:Ocean freight
Product Introduction
Low temperature container plate produced in China 12Cr1MoVR Impact temperature 20℃
Lower yield strength ReL/MPa ≥245 (T/mm 6~60) ≥235 (T/mm 60~100)
Tensile strength Rm/MPa 440~590 (T/mm 6~60) 430~580 (T/mm 60~100)
Tensile strength Rm/MPa 440~590 (T/mm 6~60) 430~580 (T/mm 60~100)
Elongation after fracture A/% ≥19
Impact absorption energy KV₂/J ≥47
Specification/mm:T (6~80+)*W*L