Detalles esenciales
Envío:海运
Introducción del producto
Low temperature container plate produced in China 18MnMoNbR Impact temperature 0℃
Lower yield strength ReL/MPa ≥400 (T/mm 30~60) ≥390 (T/mm 60~100)
Tensile strength Rm/MPa 570~720 (T/mm 30~60) 570~720 (T/mm 60~100)
Tensile strength Rm/MPa 570~720 (T/mm 30~60) 570~720 (T/mm 60~100)
Elongation after fracture A/% ≥18
Impact absorption energy KV₂/J ≥47
Specification/mm:T (6~80+)*W*L