Detalles esenciales
Envío:海运
Introducción del producto
Low temperature container plate produced in China 07Cr2AlMoR Impact temperature 20℃
Lower yield strength ReL/MPa ≥260 (T/mm 6~36) ≥250 (T/mm 36~60)
Tensile strength Rm/MPa 420~580 (T/mm 6~36) 410~570 (T/mm 36~60)
Tensile strength Rm/MPa 420~580 (T/mm 6~36) 410~570 (T/mm 36~60)
Elongation after fracture A/% ≥21
Impact absorption energy KV₂/J ≥47
Specification/mm:T (6~80+)*W*L